Glass Transition Temp, Tg 93.0 °C
199 °F
Dry; DMA
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 120 E-Glass Reinforced
Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f..
Glass Transition Temp, Tg 93.0 °C
199 °F
Dry; DMA
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f..
Glass Transition Temp, Tg 93.0 °C
199 °F
Dry; DMA
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 7581 E-Glass Reinforced
Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f..
Glass Transition Temp, Tg 93.0 °C
199 °F
Dry; DMA
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f..
Glass Transition Temp, Tg 93.0 - 153 °C
199 - 307 °F
Average value: 131 °C Grade Count:6
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Glass Transition Temp, Tg 93.0 °C
199 °F
TMA
Lord Adhesives Thermosetâ„¢ MD-150 Conductive Adhesive
LORD Thermosetâ„¢ MD-150 silver-filled conductive adhesive offers excellent electrical and thermal conductivity. It is designed for use with automated dispensing, stamping and screen-printing app..
Glass Transition Temp, Tg 93.0 °C
199 °F
wet
Henkel Hysol EA 9628H Film Adhesive
First generation, modified epoxy film, high peel strength, good stress, environmental resistance and structural propertiesApplications: Composite Bonding, Metal & Honeycomb BondingData from .060 psf..
Glass Transition Temp, Tg 93.0 °C
199 °F
wet
Henkel Hysol EA 9896 WPP Peel Ply
Pre-impregnated, nylon peel ply product supplied in film form. Specially designed resin system capable of curing at 250°F / 121°C. Compatible with state-of-the-art composite prepreg resin syst..
Glass Transition Temp, Tg 93.0 °C
199 °F
Ultimate Tg
Tra-Con Tra-Bond 2112 Rigid Epoxy Staking Compound
TRA-BOND 2112 is a thixotropic epoxy system recommended for critical electronic, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s..
Glass Transition Temp, Tg 93.0 °C
199 °F
Epoxyset Epoxibond EB-348 Low Expansion Epoxy Adhesive
EB-348 is a highly filled, extremely low expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensional ..
Glass Transition Temp, Tg 93.0 °C
199 °F
Atom Adhesives AA-BOND 428 Epoxy Adhesive
AA-BOND 428 is a two part, heat-resistant and low exotherm, epoxy adhesive formulation. It is a 100% solid epoxy adhesive, with superior chemical resistance and shear strength. AA-BOND 428 contains ..
Glass Transition Temp, Tg 93.0 °C
199 °F
Atom Adhesives AA-BOND 2112 Epoxy Adhesive
AA-BOND 2112 is a thixotropic epoxy system recommended for critical electronics, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s..