Polymer Property : Glass Transition Temp, Tg = 259 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 126 °C
259 °F
Ultimate Tg
Tra-Con Tra-Bond 526M01 Rigid Thixotropic Adhesive
TRA-BOND 526M01 is two-component, rigid, thixotropic material developed specifically for fiber optic applications. The material is a cream color when mixed and changes to a red amber color when full..
Glass Transition Temp, Tg 126 °C
259 °F
Ultimate Tg
Tra-Con Tra-Bond 789-3 Moisture Resistant Adhesive
TRA-BOND 789-3 one component, high strength toughened adhesive is designed for microelectronic applications, including substrate attach and package sealing, which require good moisture resistance. I..
Glass Transition Temp, Tg 126 °C
259 °F
Ultimate Tg
Tra-Con Tra-Bond 789-3TN1 Moisture Resistant Adhesive
TRA-BOND 789-3TN1 adhesive is a thixotropic version of TRA-BOND 789-3. It is a one component, high strength, toughened adhesive designed for use in applications which require good moisture resistanc..
Glass Transition Temp, Tg 126 °C
259 °F
10°C/min test
Polimeri Europa SINKRAL D160 ABS, Heat Stabilized  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,115-08-09-25 Very high heat injection moulding grade with good flow. Permits production of complex, thin walled..