Polymer Property : Glass Transition Temp, Tg = 3.50 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 3.50 °C
38.3 °F
DMA method 1 Hz
BorsodChem ONGRO CPE 4002 N Chlorinated Polyethylene
IMPACT MODIFIER FOR PVChigh impact resistancegood processabilityexcellent weather resistanceELASTOMERSvariety of cross-linking technologiesexcellent ozone- and weather resistanceexcellent chemical r..