Glass Transition Temp, Tg >= 162 °C
>= 324 °F
Onset; ISO 11357
Victrex® ST™ P45 PolyEtherKetoneEtherKetoneKetone (PEKEKK),
High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, coarse powder for extrusion compounding, low flow, color natural.Information Provid..
Glass Transition Temp, Tg 162 °C
324 °F
Onset; ISO 11357
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, ..
Glass Transition Temp, Tg 162 °C
324 °F
Onset; ISO 11357
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c..
Glass Transition Temp, Tg 162 °C
324 °F
Onset; ISO 11357
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, ..
Glass Transition Temp, Tg 162 °C
324 °F
ISO 11357-2
Menzolit Menzolit® BMC 1100 Unsaturated Polyester UP
BMC 1100 is a special BMC for high strength application. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. The selection of the r..
Glass Transition Temp, Tg 162 °C
324 °F
ISO 11357-2
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP
SMC 1100 is a special vinylester SMC for high strength applications. The reinforcement has been put to a level that combines mouldability with high strength and stiffness properties. The specific re..
Glass Transition Temp, Tg 162 °C
324 °F
ISO 11357-2
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP
SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc..
Glass Transition Temp, Tg 162 °C
324 °F
ISO 11357-2
Menzolit Menzolit® BMC 1400 Unsaturated Polyester UP
BMC 1400 is a special BMC for the use on an engine. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The product has been developped f..
Glass Transition Temp, Tg 162 °C
324 °F
ISO 11357-2
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP
HPC 1200 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc..
Glass Transition Temp, Tg 162 °C
324 °F
ISO 11357-2
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP
HPC 1300 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc..
Glass Transition Temp, Tg 162 °C
324 °F
D3418
Ensinger Tecapeek® ST PolyEtherKetoneEtherKetoneKetone, Unreinforced
TECAPEEK® ST is a multipurpose semi-crystaline material from the polyaryletherketone family based on PEKEKK that features improved mechanical properties at higher temperatures. The benefits of TECA..