Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 170 °C | 338 °F | Wet; DMA |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 12K PW HTS Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | Wet; DMA |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 3K PW G30-500 Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | Wet; DMA |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, IM7 Unitape Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0160 Unsaturated Polyester UP BMC 0160 is a general purpose BMC for electrical applications. Typical applications are lamp housings, canopies, covers and similar components.Information Provided by Menzolit |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0170 Unsaturated Polyester UP BMC 0170 is a general purpose BMC for electrical applications. Product according to type 801 DIN 16911. The glass content is on a level that combines good mouldability with good strength and stiffne.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0180 Unsaturated Polyester UP BMC 0180 is a general purpose BMC for electrical applications. Product according to type 803 DIN 16911. The glass content is on a level that combines good mould ability with good strength and stiffn.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0400 Unsaturated Polyester UP BMC 0400 is a low profile DMC/BMC for automotive applications. It fulfills the requirements of the automotive industry regarding painted body panels including reduced C-emissions. For highest surfac.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 1650 Unsaturated Polyester UP BMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP SMC 0180 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0200 Unsaturated Polyester UP SMC 0200 is a general purpose SMC for a wide range of applications. Typically, it is used as housings, covers and functional components in mechanical engineering. The flammability meets the demands .. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP SMC 0600 is a specially formulated SMC for reduced moulding pressure (< 30 bar). The glass level has been selected to combine good mouldability with strength and stiffness. Even without a specific f.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0650 Unsaturated Polyester UP SMC 0650 Low pressure SMC for large panels when moulding force becomes critical. Specific moulding pressure < 20 bar. A Special molding procedure is necessary.Information Provided by Menzolit |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 1600 Unsaturated Polyester UP SMC 1600 is a special SMC for sanitary applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The material shows an increased resis.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 1650 Unsaturated Polyester UP SMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0300 Unsaturated Polyester UP BMC 0300 is a low shrink standard material for general-purpose applications, which require a higher level on surface quality and better dimensional stability. The glass content is on a level that co.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 2600 Unsaturated Polyester UP BMC 2600 is a special BMC with reduced electrical properties. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. Because of its improved.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 2800 Unsaturated Polyester UP BMC 2800 is a high performance BMC for matching the demands of medium and high voltage applications in the electrical field especially in respect of RTI 160+ according to Underwriters Laboratories .. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 2900 Unsaturated Polyester UP BMC 2900 is a specially designed BMC to meet the EC Safety Signs Directive (92/58/EEC) on the provision and use of safety signs at work. In areas where it is not possible to include the use of illu.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 3000 Unsaturated Polyester UP BMC 3000 is a special BMC suitable for the use in microwave and cookware applications.It has high temperature resistance, and meets requirements for food contact applications. It has a high gloss fi.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets .. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP SMC 0290 is a specially formulated SMC processable by injection moulding. The gentle production process prevents the fiber from any damage. Parts made of SMC 0290 reach higher levels of strength and.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0300 Unsaturated Polyester UP SMC 0300 is a low shrink standard SMC providing improved surface quality, reduced shrinkage and warpage. Typical fields of applications are mechanical engineering and electrical industry, where impr.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 2500 Unsaturated Polyester UP SMC 2500 is a special SMC for high voltage isolating applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Even without a specific.. |
|||
Glass Transition Temp, Tg | >= 170 °C | >= 338 °F | |
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | 10°C/min |
Arkema Group Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Dry) Designation ISO 1874-PA12/xx,M,12-020Semi-aromatic polyamide (PASA) grade for injection molding.Transparency even thick. Outstanding thermal properties due to its high glass temperature. Good chemic.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | TMA; Nominal; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | TMA; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | DMA Method; IPC-TM-650 2.4.24 |
Rogers Corporation 2929 Bondply Unreinforced, Hydrocarbon based Thin Film Adhesive System Low dielectric constant and loss tangentIdeal for multi-layer bondingCompatible with traditional processing methodsCompatible with a broad range of material types including PTFE compositesReliable t.. |