Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, Flame Retardant , Nylon, Aromatic
Manufacturer Arkema
Trade Name Cristamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA12/xx,M,12-020Semi-aromatic polyamide (PASA) grade for injection molding.Transparency even thick. Outstanding thermal properties due to its high glass temperature. Good chemical resistance. Dimensional stability.Example applications: Oil casing.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Water Absorption 3.2 %
3.2 %
High Load Melt Index 4.9 g/10 min

@Load 21.6 kg,
Temperature 235 °C
4.9 g/10 min

@Load 47.6 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 78.0 MPa
11300 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 8.0 %
8.0 %
50 mm/min
Tensile Modulus 2.11 GPa
306 ksi
1 mm/min
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 170 °C
338 °F
10°C/min
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
Oxygen Index 26 %
26 %
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.
Users viewing this material also viewed the following: