Glass Transition Temp, Tg 35.0 °C
95.0 °F
TM R050-25
Resinlab® EP1121-4 Adhesive / Casting Resin
Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives ..
Glass Transition Temp, Tg 35.0 - 37.0 °C
95.0 - 98.6 °F
DMA, E
Proto3000 Objet DurusWhite FullCure430 Polypropylene-like Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Glass Transition Temp, Tg 35.0 °C
95.0 °F
Polynorbornene Rubber (PNR)
High glass temperature - plasticizer needed to make a 'rubbery' compound.
Glass Transition Temp, Tg 35.0 °C
95.0 °F
Mallard Creek Polymers ROVENE® 6017 Styrene-Acrylic Emulsion
ROVENE® 6017 is a stiff, self-crosslinking styrene-acrylic copolymer emulsion with excellent water resistance and good mechanical stability.APPLICATIONS: ROVENE® 6017 is recommended for bondin..
Glass Transition Temp, Tg 35.0 °C
95.0 °F
Lucite International Elvacite ® 2046 Acrylic Resin
Elvacite® 2046 is a high molecular weight iso-butyl / n-butyl methacrylate copolymer. Elvacite® 2046 is useful in aluminum finishes, ceramic coatings, and aerosol snows. It is soluble in miner..
Glass Transition Temp, Tg >= 35.0 °C
>= 95.0 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Epoxy Technology EPO-TEK® 305 Spectrally Transparent Epoxy
Product Description: EPO-TEK® 305 is a two component, semi-rigid, optical grade epoxy for semiconductor packaging of fiber optics, optoelectronics and medical devices. It is an electrically and th..
Glass Transition Temp, Tg 35.0 °C
95.0 °F
Asahi Glass Lumiflon LF-302 Solvent Soluble Fluoropolymer w/ Melamine hardening agent
Lumiflon was developed by Asahi Glass in 1982, and is unique being the first solvent soluble fluoropolymer. The FEVE based Lumiflon has a alternative copolymer. The complete inter-changeability betw..
Glass Transition Temp, Tg 35.0 °C
95.0 °F
Unitika elitel UE3500 Polyester, Flake
High molecular weight, High toughness, High strength, High elongationUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from produc..