Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glass Transition Temp, Tg = 387 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 197 °C
387 °F
TM650 2.4.25
Premix Thermoplastics PREBOARD E1026 Standard Epoxy Circuit Boards
PREBOARD is a thermoplastic based PCB laminate. Low dissipation factor leads to high gain in the antennas. As a non filled laminate PREBOARD is fully homogenous so that consistant properties are ac..
Glass Transition Temp, Tg 197 °C
387 °F
Hexcel® HexPly® 954-3A Curing Cyanate Resin
HexPly® 954-3A is a 350°F (177°C) curing cyanate resin with a 400°F (204°C) glass transition temperature. Standard cure is two hours at 350°F (177°C). Glass transition temperatures can be max..
Glass Transition Temp, Tg 197 °C
387 °F
EN6032
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/35%/UD134/AS7-12K
Fiber: AS7, Weave: UD, 134 g/m2Information provided by HexCel
Glass Transition Temp, Tg 197 °C
387 °F
Dry
Hexcel® F161 Epoxy Resin
F161 is a structural, heat resistant and electrical grade epoxy formulation designed for autoclave curing. F161 is a high temperature, laminate grade epoxy resin with a 350ºF (177ºC) cure. F161 is..
Copyright © lookpolymers.com All Rights Reserved