Hexcel® F161 Epoxy Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® F161 Epoxy Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
F161 is a structural, heat resistant and electrical grade epoxy formulation designed for autoclave curing. F161 is a high temperature, laminate grade epoxy resin with a 350ºF (177ºC) cure. F161 is unique in that it was the first resin system to meet all types and classes of MIL-R-9300 B.Uncured: Moderate viscosity during cure, Adaptable to offer good tack and drape for processing, Can be adapted for use on various weaves and fiber reinforcements, Nonburning system available (Bromine added);Cured: Heat resistant properties, Excellent heat aging properties (adaptable to tooling), Electrical grade formulation, Certified to MIL-R-9300 B (Types 1 and II, Grades O and D, Form B)
Physical Properties Metric English Comments
Specific Gravity 1.243 g/cc
1.243 g/cc
Moisture Absorption at Equilibrium 2.8 %
2.8 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
Elongation at Yield 2.2 %
2.2 %
Tensile Modulus 3.59 GPa
521 ksi
Fracture Toughness 0.433 MPa-m½
0.394 ksi-in½
Thermal Properties Metric English Comments
CTE, linear 46.8 µm/m-°C
26.0 µin/in-°F
Glass Transition Temp, Tg 152 °C
306 °F
Wet
197 °C
387 °F
Dry
Processing Properties Metric English Comments
Gel Time 1.00 - 7.00 min

@Temperature 177 °C
1.00 - 7.00 min

@Temperature 351 °F