Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -83.0 - 71.0 °C | -117 - 160 °F | Average value: -34.4 °C Grade Count:34 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |
|||
Glass Transition Temp, Tg | 20.0 - 71.0 °C | 68.0 - 160 °F | Average value: 54.2 °C Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |