Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glass Transition Temp, Tg = 68.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 20.0 °C
68.0 °F
Mallard Creek Polymers Rovene® 6025 Styrene-Acrylic Emulsion
Applications: Rovene® 6025 can be used in multiple coating and paint applications including landscaping coatings and low sheen interior flat wall coatings. It can also be used as a binder for dus..
Glass Transition Temp, Tg 20.0 °C
68.0 °F
Mallard Creek Polymers Rovene® 6102 Resin Supported Emulsion
Rovene® 6102 is a hard, film forming vehicle with a moderately low glass transition temperature (Tg) for flexographic and gravure inks and overprint varnishes, that exhibits good water resistance..
Glass Transition Temp, Tg 20.0 °C
68.0 °F
Mallard Creek Polymers Rovene® 6112 Resin Supported Emulsion
Rovene® 6112 is a hard, film forming, low glycol ether and VOC vehicle with a moderately low glass transition temperature for flexographic and gravure inks and overprint varnishes. Rovene® 611..
Glass Transition Temp, Tg 20.0 °C
68.0 °F
Mallard Creek Polymers Rovene® 6126 Styrene-Acrylic Emulsion
Applications: Rovene® 6126 provides a flexible yet strong cohesive bond for a range of materials and particle surface areas. Rovene® 6126 imparts films with good water resistance properties. F..
Glass Transition Temp, Tg 20.0 °C
68.0 °F
Mallard Creek Polymers Tykote® 6152 Styrene-Acrylic Emulsion
Tykote® 6152 is a hard film forming styrene-acrylic emulsion designed for oil and grease resistant barrier coatings. This product also provides excellent water and blocking resistance in barrier ..
Glass Transition Temp, Tg 20.0 °C
68.0 °F
Lucite International Elvacite ® 2044 Acrylic Resin
Elvacite® 2044 is a high molecular weight n-butyl methacrylate polymer. Elvacite® 2044 is useful in adhesives for smooth plastic films and aluminum, and in silk screen inks. It will plasticize..
Glass Transition Temp, Tg 20.0 °C
68.0 °F
Styron XZ 97212.00 Functionalized SB
Performance Features: High stiffness, high mechanical stability, self cross-linking, low HCHO applicationsApplications: Fiber Binding, Glass Fiber Binding and NonwovensEuropeInformation provided by ..
Glass Transition Temp, Tg 20.0 °C
68.0 °F
Ultimate Tg
Tra-Con Tra-Duct 926H01
Information provided by Tra-Con Inc.
Glass Transition Temp, Tg >= 20.0 °C
>= 68.0 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Epoxy Technology EPO-TEK® EE165-3 Silver Filled Epoxy
A two component, silver-filled, electrically conductive epoxy made for bonding of SMDs, and general solder replacement at the PCB level and circuit assembly. It was designed to be low modulus and f..
Glass Transition Temp, Tg >= 20.0 °C
>= 68.0 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
Epoxy Technology EPO-TEK® H20F Electrically Conductive, Flexible Epoxy
Product Description: EPO-TEK® H20F is a two component, flexible silver epoxy. It was designed for flexible type circuitry, such as switching circuits in a flexible panel system, as well as large di..
Glass Transition Temp, Tg >= 20.0 °C
>= 68.0 °F
Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Epoxy Technology EPO-TEK® T7109-17 Thermally Conductive Epoxy
Product Description: EPO-TEK® T7109-17 is a flexible, thermally conductive, electrically insulating epoxy paste designed for low stress and heat dissipation applications within the semiconductor, h..
Glass Transition Temp, Tg 20.0 °C
68.0 °F
LookPolymers® 2550 100% Acrylic Emulsion for Paint
Information provided by Celanese Emulsion Polymers.
Glass Transition Temp, Tg 20.0 °C
68.0 °F
LookPolymers® 7305 Vinyl Acrylic Emulsion for Paint
Information provided by Celanese Emulsion Polymers.
Glass Transition Temp, Tg 20.0 °C
68.0 °F
ISO 11357-1,-2,-3
3425HRT PBT, Glass Reinforced
Celanex 3425HRT is a non-lubricated, 40% fiberglass reinforced PBT copolymer that has excellent hydrolysis resistance, toughness, improved flow, and improved elongation at break.Information provided..
Glass Transition Temp, Tg 20.0 °C
68.0 °F
LookPolymers® 1063 PVAc Emulsion for Building Products
Information provided by Celanese Emulsion Polymers.
Glass Transition Temp, Tg 20.0 °C
68.0 °F
Mid-Point
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro..
Glass Transition Temp, Tg 20.0 °C
68.0 °F
LookPolymers® 7448 Vinyl Acrylic Emulsion for Paint
Information provided by Celanese Emulsion Polymers.
Glass Transition Temp, Tg 20.0 °C
68.0 °F
Loctite® Durabond® E-00CL Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..
Glass Transition Temp, Tg 20.0 °C
68.0 °F
Loctite® Durabond® E-00NS Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..
Glass Transition Temp, Tg 20.0 °C
68.0 °F
for homopolymer
Solvay SIPOMER® PAM-100 Phosphate Esters of Polyethylene Glycol Monomethacrylate
Description: Sipomer PAM-100 incorporated into acrylic or styrene acrylic latex systems improves adhesion to metallic substrates and glass. Sipomer PAM-100 also enhances properties such as freeze/th..
Glass Transition Temp, Tg 20.0 - 71.0 °C
68.0 - 160 °F
Average value: 54.2 °C Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..
Copyright © lookpolymers.com All Rights Reserved