Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 72.2 °C | 162 °F | Tg onset, Dry, Cured Neat Resin Property, 1 hour @ 70°C/158°F |
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and .. |