Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 72.0 °C | 162 °F | Dynamic Viscoelasticity |
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas .. |
|||
Glass Transition Temp, Tg | 72.0 °C | 162 °F | ISO 11359-2:1999 |
Global EPP PA 66E Extruded Polyamide 66 Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecu.. |
|||
Glass Transition Temp, Tg | 72.0 °C | 162 °F | Ultimate Tg |
Tra-Con Tra-Bond 723C01 One-Part Medical Grade Adhesive TRA-BOND 723C01 is a fast, heat curing, one component adhesive targeted at medical applications. The material complies with USP Class VI toxicity requirements and is resistant to gamma sterilization.. |
|||
Glass Transition Temp, Tg | 72.0 °C | 162 °F | ASTM E1545-11 |
DSM Somos® PerFORM Stereolithography Polymer, UV Postcure PerFORM produces strong, stiff, high-temperature resistant composite parts on standard 355 nm stereolithography machines. This material’s lower viscosity makes processing parts faster. It exhibits .. |
|||
Glass Transition Temp, Tg | 72.0 °C | 162 °F | 10 K/min; ISO 11357-1/-3 |
BASF Ultramid® A27 E 01 PA66 (Dry) Ultramid A27 E 01 is a low-viscosity, general-purpose PA66 grade for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation ".. |
|||
Glass Transition Temp, Tg | 72.0 °C | 162 °F | |
Unitika elitel UE3600 Polyester, Pellet High Tg, PET adhesiveness, Transparency, BinderUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, .. |
|||
Glass Transition Temp, Tg | 72.2 °C | 162 °F | Tg onset, Dry, Cured Neat Resin Property, 1 hour @ 70°C/158°F |
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and .. |