Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 73.9 °C | 165 °F | |
Gromax Evasin EV-3201V Ethylene-Vinyl Alcohol Copolymer Unmodified random Co-Polymer of [Ethylene-Vinyl alcohol], designed for therm-plastic processing into Sheets and Foils with high Oxygen and Aroma Barrier EffectInformation provided by Gromax Enterpri.. |