Thermal Properties Metric English Comments
Glass Transition Temp, Tg 81.1 °C
178 °F
ASTM D3418
Plaskolite Vivak PETG Sheet
VIVAK offers a balance of physical properties and ease of fabrication. It is ideally suited for complex parts requiring fabrication, including deep thermoforming draws and precise molded-in details...