Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 29.0 °C | 84.2 °F | DSC; ASTM E1356-03 |
NeXolve UV Blocking Optionox® Polyimide Film/Coating Highly UV durable with excellent weatherability and stability to ozone.Optinox® films and coatings are highly UV durable and exhibit excellent weathering durability, including very high stability .. |
|||
Glass Transition Temp, Tg | 29.0 °C | 84.2 °F | Mid-point |
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb.. |