Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 94.0 °C | 201 °F | |
Hybrid Plastics Nanoreinforced® Cellulose Propionate Acetate Nanoreinforced® Cellulose Propionate Acetate is an optically clear nanocomposite with POSS® dispersed at the nanometer level. Compared to virgin cellulose propionate acetate, it enhances mecha.. |