Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 144 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 144 °C

@Thickness 6.40 mm
291 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC
LNP* Stat-kon* Lexan_LC1500N compound is a 15% carbon fiber, 6% PTFE reinforced polycarbonate.
Deflection Temperature at 0.46 MPa (66 psi) 144 °C

@Thickness 6.40 mm
291 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Europe-Africa-Middle East)
LNP* Stat-kon* Lexan_LCF1506 is a 15% carbon fiber, 6% PTFE reinforced polycarbonate.
Deflection Temperature at 0.46 MPa (66 psi) 144 °C

@Thickness 6.40 mm
291 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Asia Pacific)
15% carbon fiber, 6% PTFE reinforced polycarbonate.