Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C @Thickness 12.7 mm |
199 °F @Thickness 0.500 in |
Unannealed; ASTM-D648 |
Ineos ABS Lustran® ABS 248FC Medical & Food Contact Grade Lustran® ABS 248FC resin is a high-gloss, medium-impact grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of physical properties and has been desi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C @Thickness 3.20 mm |
199 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 93.0 °C @Thickness 6.40 mm |
199 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL HIPS3190 HIPS Complies with FDA Regulation 21 CFR 177.1640 for rubber modified polystyrene. HB rating from 0.062-0.125"" pending. Natural only. |