Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C

@Thickness 3.18 mm
190 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ HTX 92052 Polyvinyl Chloride Alloy (PVC Alloy)
Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C

@Thickness 3.18 mm
190 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ HTX Ultra LA426G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy)
Higher gloss version of Geon HTX Ultra LA426Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426G Black 2880.Information provided by Pol..
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C

@Thickness 3.18 mm
190 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ HTX Ultra LA436G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy)
Higher gloss, wider processing window version of Geon HTX Ultra LA426G.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA436G Black 2880...
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C

@Thickness 3.17 mm
190 °F

@Thickness 0.125 in
Unannealed; ASTM-D648
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)