Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 82.0 °C @Thickness 6.40 mm |
180 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® RCY6013 PC+ABS (Asia Pacific) Cycoloy* RCY6013 resin is an injection moldable high flow PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 @ 1.5 mm.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.0 °C @Thickness 6.40 mm |
180 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® RCY6113 PC+ABS (Asia Pacific) Cycoloy* RCY6113 resin is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 5VB rating @ 2.0mm an.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C @Thickness 3.18 mm |
180 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ HTX Ultra LA426 Tan 3725 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.0 °C @Thickness 12.7 mm |
180 °F @Thickness 0.500 in |
Unannealed; ASTM-D648 |
Ineos ABS Lustran® 266 ABS, Transparent Grade Lustran® ABS 266 resin is a clear injection molding grade of ABS (acrylonitrile butadiene styrene). This transparent, general-purpose grade provides clarity and toughness with ease of processing... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.0 °C @Thickness 3.20 mm |
180 °F @Thickness 0.126 in |
ASTM D648 |
LG Chemical XG568 MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.0 °C @Thickness 3.20 mm |
180 °F @Thickness 0.126 in |
ASTM D648 |
LG Chemical XG569C MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 82.2 °C @Thickness 3.20 mm |
180 °F @Thickness 0.126 in |
Unannealed; ASTM D648 |
Styron Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS) Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance to processability, impact resistance and heat resistance as imparted by the various polymer compositions... |