Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C

@Thickness 6.40 mm
196 °F

@Thickness 0.252 in
ASTM D648
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow
Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C

@Thickness 3.20 mm
196 °F

@Thickness 0.126 in
ASTM D648
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow
Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical