Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
ASTM D648 |
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
ASTM D648 |
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical |