Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 94.0 °C @Thickness 3.20 mm |
201 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycolac® X15 ABS Automotive. Very high heat resistance with high impact. UL94 HB rated. High gloss.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 94.0 °C @Thickness 6.40 mm |
201 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C2951 PC+ABS CYCOLOY C2951 is a flame retardant PC+ABS free from chlorinated or brominated flame retardant additives. High heat resistance is offered for demanding electrical applications, whilst maintaining exc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 94.0 °C @Thickness 12.7 mm |
201 °F @Thickness 0.500 in |
Annealed; ASTM-D648 |
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 94.0 °C @Thickness 6.40 mm |
201 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON Cycoloy_JK800 PC+ABS LNP* Stat-kon* Cycoloy_JK800 compound is an 8% carbon fiber reinforcedPC+ABS, electrostatic dissipative ECO conforming FR. Good hydrolytic stability. |