Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 94.4 °C

@Thickness 3.17 mm
202 °F

@Thickness 0.125 in
Annealed; ASTM D648
Calsak CS-72 General Purpose ABS Resin
Product Characteristics:High Impact, High GlossInjection molding grade