Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 68.9 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C

@Thickness 6.35 mm
156 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M3800 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C

@Thickness 6.35 mm
156 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5000 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C

@Thickness 6.35 mm
156 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5015 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C

@Thickness 3.18 mm
156 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5705 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C

@Thickness 6.35 mm
156 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding MR900 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C

@Thickness 6.35 mm
156 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ HC 8210 Polyvinyl Chloride, Rigid (PVC, Rigid)
Geon HC 8210 is a high flow, high impact resistance rigid grade offering enhanced chemical resistance for medical device housing applications. It is RoHS compliant with UL V0 and 5VA ratings.Informa..
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C

@Thickness 6.35 mm
156 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy)
Information provided by PolyOne