Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C @Thickness 3.18 mm |
183 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ HTX Ultra LA425 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors below 50L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Ductile/Brittle transition as measured by Instrumented Impact is 5 de.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.9 °C @Thickness 3.18 mm |
183 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ HTX Ultra LA426 Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426 Black 2880.Information provided by PolyOne |