Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 87.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C

@Thickness 3.20 mm
189 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® C2950HF PC+ABS
Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced impact and heat properties plus improved flow for various applications.
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C

@Thickness 3.20 mm
189 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Asia Pacific)
Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs.
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C

@Thickness 3.20 mm
189 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS
Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs.
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C

@Thickness 6.40 mm
189 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical HF380I ABS, High Flow
Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C

@Thickness 6.40 mm
189 °F

@Thickness 0.252 in
ASTM D648
LG Chemical HI100 ABS, High Impact
Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C

@Thickness 6.40 mm
189 °F

@Thickness 0.252 in
ASTM D648
LG Chemical HI100K ABS, High Impact
Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C

@Thickness 6.40 mm
189 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical HT700 ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C

@Thickness 12.7 mm
189 °F

@Thickness 0.500 in
Unannealed; ASTM-D648
Ineos ABS Lustran® 308 ABS, Medical Grade
Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi..
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C

@Thickness 6.40 mm
189 °F

@Thickness 0.252 in
unannealed; ASTM D 648
SABIC Innovative Plastics Noryl N190A PPE+PS (Asia Pacific)
Low heat, flame retardant PPO/HIPS alloy. Internal flammability results only.Not a UL recognised material.This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C

@Thickness 6.40 mm
189 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow
Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C

@Thickness 3.20 mm
189 °F

@Thickness 0.126 in
Unannealed; ASTM D648
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow
Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical