SABIC Innovative Plastics Noryl N190A PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Noryl N190A PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low heat, flame retardant PPO/HIPS alloy. Internal flammability results only.Not a UL recognised material.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D 792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
Type I, 50 mm/min; ASTM D 638
Elongation at Break 41 %
41 %
Type I, 50 mm/min; ASTM D 638
Flexural Yield Strength 55.0 MPa
7980 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2.20 GPa
319 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 1.97 J/cm

@Temperature 23.0 °C
3.69 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 130 µm/m-°C

@Temperature -40.0 - 60.0 °C
72.2 µin/in-°F

@Temperature -40.0 - 140 °F
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 3.20 mm
178 °F

@Thickness 0.126 in
unannealed; ASTM D 648
87.0 °C

@Thickness 6.40 mm
189 °F

@Thickness 0.252 in
unannealed; ASTM D 648
Vicat Softening Point 95.0 °C
203 °F
Rate B/50; ASTM D 1525
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
UL 94 by SABIC-IP