Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 126 µm/m-°C

@Temperature -30.0 - 30.0 °C
70.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP ML004 PP
LNP* LUBRICOMP* ML004 is a product based on Polypropylene containing 20% PTFE. Added features of this grade include: Wear Resistant.
CTE, linear, Transverse to Flow 126 µm/m-°C

@Temperature -30.0 - 30.0 °C
70.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON MX12407C PP
LNP* STAT-KON* MX12407C is a compound based on Polypropylene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System.
CTE, linear, Transverse to Flow 126 µm/m-°C

@Temperature -30.0 - 30.0 °C
70.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-LOY AX11421 ABS
LNP* STAT-LOY* AX11421 is a compound based on ABS resin. Added feature of this material is: Antistatic.
CTE, linear, Transverse to Flow 126 µm/m-°C

@Temperature 26.0 - 200 °C
70.0 µin/in-°F

@Temperature 78.8 - 392 °F
ASTM D696
Saint-Gobain Fluoroloy® A16 High Performance Seal Material
General purpose material for heat and wear resistance; Recommended for dry and poorly lubricated applications; Particularly suitable for water and steam service Information provided by Saint-Goba..
CTE, linear, Transverse to Flow 126 µm/m-°C

@Temperature 23.0 - 60.0 °C
70.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP MF006SXP PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MF006SXP is a compound based on Polypropylene resin containing Glass Fiber. Added features include: Chemically Coupled.
CTE, linear, Transverse to Flow 126 µm/m-°C

@Temperature 20.0 °C
70.0 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® RS 6030 AT Nylon 6 Alloy, 30% Glass Fiber (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties...
CTE, linear, Transverse to Flow 126 µm/m-°C

@Temperature 20.0 °C
70.0 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® RS 6030 Nylon 6 Alloy, 30% Glass Fiber (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties..