Arkema Group Orgalloy® RS 6030 AT Nylon 6 Alloy, 30% Glass Fiber (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Arkema
Trade Name Orgalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Orgalloy® RS 6030 AT Nylon 6 Alloy, 30% Glass Fiber (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.30 % glass filled, conductive, for injection molding of technical parts and for extrusion of profiles.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
Water Absorption 2.3 %
2.3 %
Moisture Absorption at Equilibrium 0.90 %
0.90 %
Humidity Absorption
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 235 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 120 MPa
17400 psi
5 mm/min
Elongation at Break 3.5 %
3.5 %
5 mm/min
Tensile Modulus 7.50 GPa
1090 ksi
1 mm/min
Charpy Impact, Notched 0.550 J/cm²
2.62 ft-lb/in²
Tensile Creep Modulus, 1 hour 5740 MPa
833000 psi
Tensile Creep Modulus, 1000 hours 4050 MPa
587000 psi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 20.0 °C
10.6 µin/in-°F

@Temperature 68.0 °F
CTE, linear, Transverse to Flow 126 µm/m-°C

@Temperature 20.0 °C
70.0 µin/in-°F

@Temperature 68.0 °F
Melting Point 220 °C
428 °F
10°C/min
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
Vicat Softening Point 183 °C
361 °F
50°C/hr; 50N
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Electrical Resistivity 430000 ohm-cm
430000 ohm-cm
Surface Resistance 55000 ohm
55000 ohm