Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 152 µm/m-°C

@Temperature 23.0 - 60.0 °C
84.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE (Europe-Africa-Middle East)
LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing PTFE.
CTE, linear, Transverse to Flow 152 µm/m-°C

@Temperature 26.0 - 200 °C
84.4 µin/in-°F

@Temperature 78.8 - 392 °F
ASTM D696
Saint-Gobain Fluoroloy® A01 High Performance Seal Material
Excellent for light dynamic and static service; Limited wear and heat resistance; Low gas permeability; Good cryogenic properties; Moderate to hard vacuum service; FDA approved. Information provide..
CTE, linear, Transverse to Flow 152 µm/m-°C

@Temperature 23.0 - 200 °C
84.4 µin/in-°F

@Temperature 73.4 - 392 °F
ASTM D696
Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static)
Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Electrical: Ideal for Anti - Static Applications; Anti -..
CTE, linear, Transverse to Flow 152 µm/m-°C

@Temperature 23.0 - 200 °C
84.4 µin/in-°F

@Temperature 73.4 - 392 °F
ASTM D696
Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static)
Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Electrical: Ideal for Anti - Static Applications; Anti -..