Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Electrical: Ideal for Anti - Static Applications; Anti - Static Hose Linings; and Anti - Static Diaphragms.CHEMICAL RESISTANCE: The strength of the carbon - fluorine bond and the shielding of the carbon chains by the fluorine atoms result in a chemical inertness which is virtually universal, except alkali metals, fluorine under certain conditions, and some fluorine compounds at elevated temperatures. Some Fluorinated Hydrocarbons (refrigerants) cause reversible swelling i.e. Telrafluorodichloroethane Frigen 21, giving a 9.6% weight increase. For specific data on chemical resistance of this material we have a computer database with all the information covering over 90% of all known chemicals.Information provided by Dalau
Physical Properties Metric English Comments
Density 2.13 - 2.19 g/cc
0.0770 - 0.0791 lb/in³
BS2782:Pt6
Deformation 7.9 %
7.9 %
Permanent Deformation; ASTM D621
10 %

@Time 3600 sec,
Pressure 5.00 MPa
10 %

@Time 1.00 hour,
Pressure 725 psi
150°C; ASTM D621
11.8 %

@Time 3600 sec,
Pressure 14.2 MPa
11.8 %

@Time 1.00 hour,
Pressure 2060 psi
ASTM D621
14.3 %

@Pressure 14.2 MPa,
Time 86400 sec
14.3 %

@Pressure 2060 psi,
Time 24.0 hour
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 57 - 64
57 - 64
ASTM D2240
Tensile Strength 20.0 - 35.0 MPa
2900 - 5080 psi
Moulding Direction; BS2782:Pt3
Elongation at Break 150 - 350 %
150 - 350 %
Moulding Direction; BS2782:Pt3
Flexural Modulus 0.690 GPa
100 ksi
ASTM D790
Coefficient of Friction, Dynamic 0.060
0.060
ASTM D1894
Coefficient of Friction, Static 0.080
0.080
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 142 µm/m-°C

@Temperature 23.0 - 200 °C
78.9 µin/in-°F

@Temperature 73.4 - 392 °F
ASTM D696
CTE, linear, Transverse to Flow 152 µm/m-°C

@Temperature 23.0 - 200 °C
84.4 µin/in-°F

@Temperature 73.4 - 392 °F
ASTM D696
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
Moulding Direction; ASTM C177
Melting Point 327 °C
621 °F
ASTM D3417
Maximum Service Temperature, Air 260 °C
500 °F
300 °C
572 °F
Short Periods
Minimum Service Temperature, Air -200 °C
-328 °F
Flash Point 530 °C
986 °F
ASTM D1929
Oxygen Index >= 95 %
>= 95 %
ASTM D2863
Descriptive Properties Value Comments
Color Black