Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 59.7 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP LX00430 PEEK LNP* LUBRICOMP* LX00430 is a compound based on Pelyetheretherketone containing Proprietary Fillers. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 59.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DX09303C PC (Asia Pacific) LNP* Stat-Kon* DX09303C is carbon fiber filled polycarbonate composite with high modulus, good flow ability, and high level of cleanliness for the most demanding application. A unique feature of thi.. |