Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 85.0 - 85.0 µm/m-°C @Temperature 55.0 - 160 °C |
47.2 - 47.2 µin/in-°F @Temperature 131 - 320 °F |
Average value: 85.0 µm/m-°C Grade Count:1 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear, Transverse to Flow | 85.0 - 100 µm/m-°C | 47.2 - 55.6 µin/in-°F | Average value: 91.7 µm/m-°C Grade Count:3 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics GELOY CR7501 ASA (Europe-Africa-Middle East) High heat injection moulding grade, blend of ASA/AMSAN. It can be positioned for outside parts in various markets. Various colours. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C | 47.2 µin/in-°F | Average above Tg; ISO 11359 |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical PI-642 ABS, Fitting, High Strength Information Provided by LG Chem |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 176 PBT Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 815UX PBT (Europe-Africa-Middle East) VALOX 815UX is a 15% glass reinforced PBT+PET blend with improved surface appearance and excellent UV performance. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 (Europe-Africa-Middle East) Heat stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
47.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX951W PPE+PA66 (Asia Pacific) A new high flow GTX designed for under-the-hood applications such as power distribution boxes, relay boxes and junction boxes. Developmental name: EXNX0151. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp PF006 PA 6 (Europe-Africa-Middle East) 30% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 (Europe-Africa-Middle East) UV stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® T 85 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 .. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® T 85 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 .. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® T65 AT PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp.. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® T65 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding, easy .. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C | 47.2 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® T65 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 120 °Cgood low temperature impact strengthPreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C | 47.2 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® T65 XF Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 120 °Cimproved flowability compared to T65PreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C | 47.2 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 570 NC000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler for injection molding. Delrin 570 has very high stiff.. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG6H PA6, 30% Glass Filled, Injection Molded BG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide PF006 PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF06 is an 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 20.0 °C |
47.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® KL 1-1430 Polycarbonate/ABS Blend Standard grade for cars.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FN150 PPE+HIPS (Europe-Africa-Middle East) NORYL FN150 twin wall foam meets UL standard 94 V-0/5V ratings at 4 mm wall thickness. These unique flammability characteristics make FN150 the supreme choice for designing optimum wall thickness in.. |
|||
CTE, linear, Transverse to Flow | 85.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
47.2 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66
(Unverified Data**) Zytel® 70G35HSLX BK357 is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |