Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 50.0 - 100 µm/m-°C
27.8 - 55.6 µin/in-°F
Average value: 79.3 µm/m-°C Grade Count:15
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
CTE, linear, Transverse to Flow 85.0 - 100 µm/m-°C
47.2 - 55.6 µin/in-°F
Average value: 91.7 µm/m-°C Grade Count:3
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
CTE, linear, Transverse to Flow 27.0 - 100 µm/m-°C
15.0 - 55.6 µin/in-°F
Average value: 51.2 µm/m-°C Grade Count:10
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
CTE, linear, Transverse to Flow 3.60 - 100 µm/m-°C
2.00 - 55.6 µin/in-°F
Average value: 63.6 µm/m-°C Grade Count:9
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
CTE, linear, Transverse to Flow 76.0 - 100 µm/m-°C

@Temperature 55.0 - 260 °C
42.2 - 55.6 µin/in-°F

@Temperature 131 - 500 °F
Average value: 83.8 µm/m-°C Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
CTE, linear, Transverse to Flow 76.0 - 100 µm/m-°C

@Thickness 2.00 - 4.00 mm
42.2 - 55.6 µin/in-°F

@Thickness 0.0787 - 0.157 in
Average value: 83.8 µm/m-°C Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
CTE, linear, Transverse to Flow 34.0 - 100 µm/m-°C
18.9 - 55.6 µin/in-°F
Average value: 66.3 µm/m-°C Grade Count:24
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
CTE, linear, Transverse to Flow 50.0 - 100 µm/m-°C
27.8 - 55.6 µin/in-°F
Average value: 75.3 µm/m-°C Grade Count:8
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
CTE, linear, Transverse to Flow 60.0 - 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
33.3 - 55.6 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® C3U BK 23079 PA6/66 FR (Conditioned)
Description: Injection-molding grade with improved flame retardance (free from halogens and phosphorus), used e.g. for impact resistant electrically insulating parts such as contact bases and plug c..
CTE, linear, Transverse to Flow 70.0 - 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 55.6 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® FRee A3U40G5 25% Glass Filled PA66 FR (Dry)
Description: Flame retardant without halogens and red phosphorus, 25% glass fiber reinforced injection-molding grade; light colorable; outstanding mechanical and electrical properties.Information pr..
CTE, linear, Transverse to Flow 35.0 - 100 µm/m-°C
19.4 - 55.6 µin/in-°F
Average value: 68.7 µm/m-°C Grade Count:7
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
CTE, linear, Transverse to Flow 22.0 - 100 µm/m-°C

@Temperature -100 - 250 °C
12.2 - 55.6 µin/in-°F

@Temperature -148 - 482 °F
Average value: 81.8 µm/m-°C Grade Count:23
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..