Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 39.0 - 92.0 µm/m-°C | 21.7 - 51.1 µin/in-°F | Average value: 75.0 µm/m-°C Grade Count:10 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |