Polymer Property : CTE, linear, Transverse to Flow = 21.7 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
21.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP DFL38 PC
LNP* Lubricomp* DFL-4038 is a Polycarbonate containing 40% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated.
CTE, linear, Transverse to Flow 39.0 - 92.0 µm/m-°C
21.7 - 51.1 µin/in-°F
Average value: 75.0 µm/m-°C Grade Count:10
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
CTE, linear, Transverse to Flow 39.0 µm/m-°C
21.7 µin/in-°F
Idemitsu Kosan Xarec® D132 SPS, 25% Glass Filled
CTE, linear, Transverse to Flow 39.0 µm/m-°C
21.7 µin/in-°F
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled
Glass Filled, Ignition Resistant, Impact Modified. Used in electronic and electrical applications.
CTE, linear, Transverse to Flow 39.0 µm/m-°C
21.7 µin/in-°F
ASTM D696
Kuraray Genestarâ„¢ G1350A-M42 Nylon, 35% Glass Filled
35% Glass reinforced injection grade. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment.Main Features:Hydrolysis resistanceHeat resista..
CTE, linear, Transverse to Flow 39.0 µm/m-°C
21.7 µin/in-°F
ASTM D696
Kuraray Genestarâ„¢ GC1201A-M41 Nylon, Glass Filled and Carbon Filled
Reinforced injection grade for conductive applications.Main Features:ConductivityHeat resistanceChemical resistanceExample of applications:Quick connector
CTE, linear, Transverse to Flow 39.0 µm/m-°C
21.7 µin/in-°F
ISO 11359-1/-2
Lanxess Durethan® DP 2802/30 000000 Nylon 66, 30% Glass Fiber
PA 66 injection molding grade, 30% glass fibers, UL 94V-2 at 0.75 mm , GWFI:960°C at 0.75 mm, GWIT: 775°C at 0,75 mm, halogen-freeApplication Examples: mixer insert for blenders, washing machi..
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
21.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP OX91041 PPS - LINEAR (Europe-Africa-Middle East)
LNP* LUBRICOMP* OX91041 is a compound based on PPS Linear resin containing Carbon Fiber, Glass Fiber, PTFE. Added features include: Internally Lubricated, Electrically Conductive.
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
21.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON OE008 PPS (Europe-Africa-Middle East)
LNP * Stat-kon* OE 008 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include: Electically Conductive.
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
21.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Europe-Africa-Middle East)
LNP* THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features include: Electrically Conductive.
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
21.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp EF008EXP PEI (Europe-Africa-Middle East)
LNP* Thermocomp* EF008EXP is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SABIC-IP ..
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature 20.0 °C
21.7 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Sumitomo Bakelite North America RX® 853G Fiberglass Reinforced Phenolic Novolac
RX 853G is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am..
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature 20.0 °C
21.7 µin/in-°F

@Temperature 68.0 °F
TMA
Sumitomo Bakelite North America RX® 865M Fiberglass Reinforced Phenolic Novolac
RX 865M is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am..
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature 20.0 °C
21.7 µin/in-°F

@Temperature 68.0 °F
ASTM E-831
Sumitomo Bakelite North America RX® 865M Novolac Phenolic
Fiberglass reinforced phenolic novolac compound featuring dimensional stability, moderate impact resistance, good strength and modulus.Information provided by Vyncolit, a Sumitomo Bak Group