Polymer Property : CTE, linear, Transverse to Flow = 56.7 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 102 µm/m-°C

@Temperature 23.0 - 60.0 °C
56.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer (Europe-Africa-Middle East)
LNP* LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing milled Glass and PTFE. Added features include; Internally Lubricated.
CTE, linear, Transverse to Flow 102 µm/m-°C

@Temperature 23.0 - 60.0 °C
56.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RX94033 PA6.6 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RX94033 is a compound based on PA 66 resin containing Aramide Fiber, Glass Fiber, PTFE. Added features include: Internally Lubricated.
CTE, linear, Transverse to Flow 102 µm/m-°C

@Temperature -30.0 - 30.0 °C
56.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP VC006 SUPER TOUGH NYLON
LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon resin containing 30% Carbon Fiber. Added features of this material include: High Impact, Electrically Conductive.
CTE, linear, Transverse to Flow 102 µm/m-°C

@Temperature -30.0 - 30.0 °C
56.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT
LNP* THERMOCOMP* WF004 is a compound based on PBT resin containing 20% Glass Fiber.
CTE, linear, Transverse to Flow 102 µm/m-°C

@Temperature -30.0 - 30.0 °C
56.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOTUF VC006 Super Tough PA 6/6
LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon 6/6 resin containing Carbon Fiber. Added features of this material include: High Impact.
CTE, linear, Transverse to Flow 102 µm/m-°C

@Temperature -40.0 - 37.8 °C
56.7 µin/in-°F

@Temperature -40.0 - 100 °F
ASTM E831
Diamond Polymers DIAMALOY GLY FXW749 Sheet Extrusion Grade, Sparkle/Pearlescence
Diamaloy GLY FXW749SK resin is a low impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging and added visual effects (pearlescence). It has good melt strength for..
CTE, linear, Transverse to Flow 102 µm/m-°C

@Temperature 23.0 - 60.0 °C
56.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 102 µm/m-°C

@Temperature 23.0 - 60.0 °C
56.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide BG3ST43 PA6, 15% Glass Fiber Filled, Impact Modified, Injection Molded
BG3ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Copyright © lookpolymers.com All Rights Reserved