Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers DIAMALOY GLY FXW749 Sheet Extrusion Grade, Sparkle/Pearlescence

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers DIAMALOY GLY FXW749 Sheet Extrusion Grade, Sparkle/Pearlescence.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Diamaloy GLY FXW749SK resin is a low impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging and added visual effects (pearlescence). It has good melt strength for extrusion and thermoforming, and it can be easily coextruded.Applications: Typical applications include those requiring a special visual effect, weatherability, durability, and some impact i.e., thermoformed shower stalls and pool and spa applications. As with any product, use of Diamaloy GLY FXW749SK resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 9.2 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.2 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
chs 2.0 in/min; ASTM D638
Tensile Strength, Yield 54.0 MPa
7830 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 8.5 %
8.5 %
chs 2.0 in/min; ASTM D638
Elongation at Yield 2.9 %
2.9 %
chs 2.0 in/min; ASTM D638
Flexural Strength 85.0 MPa

@Thickness 3.17 mm
12300 psi

@Thickness 0.125 in
chs 0.05 in/min; 2 in span; ASTM D790
Flexural Modulus 2.921 GPa

@Thickness 3.17 mm
423.7 ksi

@Thickness 0.125 in
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Impact Test 3.62 J
2.67 ft-lb
Total Energy; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature -40.0 - 37.8 °C
50.0 µin/in-°F

@Temperature -40.0 - 100 °F
ASTM E831
CTE, linear, Transverse to Flow 102 µm/m-°C

@Temperature -40.0 - 37.8 °C
56.7 µin/in-°F

@Temperature -40.0 - 100 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
0.125";; ASTM D648
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525