Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 57.6 µm/m-°C @Temperature -30.0 - 30.0 °C |
32.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RX06480 PA 66 LNP LUBRICOMP* RX06480 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% Lubricants. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 57.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 57.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
32.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend (Asia Pacific) LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant. |