SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ISO 1183
1.54 g/cc
0.0556 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Time 86400 sec
0.0010 - 0.0030 in/in

@Time 24.0 hour
ASTM D955
0.0010 - 0.0030 cm/cm

@Time 86400 sec
0.0010 - 0.0030 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
ASTM D638
119 MPa
17300 psi
ISO 527
Elongation at Break 0.90 %
0.90 %
ASTM D638
1.2 %
1.2 %
ISO 527
Tensile Modulus 11.53 GPa
1672 ksi
50 mm/min; ASTM D638
11.69 GPa
1695 ksi
1 mm/min; ISO 527
Flexural Strength 192 MPa
27800 psi
ISO 178
199 MPa
28900 psi
ASTM D790
Flexural Modulus 9.90 GPa
1440 ksi
ISO 178
11.45 GPa
1661 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.23 J/cm
9.80 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 57.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
32.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 262 °C
504 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
263 °C

@Thickness 3.20 mm
505 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.55 mm
V-0

@Thickness 0.0610 in
UL 94 by SABIC-IP