Polymer Property : CTE, linear, Transverse to Flow = 7.00 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 12.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
7.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON 9X06519 Cyclic Olefinic Copolymer
LNP STAT-KON* 9X06519 is a compound based on Cyclic Olefinic Copolymer resin containing 30% Carbon Fiber. Added features of this material include: Clean Compounding System, Electrically Conductive...
CTE, linear, Transverse to Flow 12.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
7.00 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON 9X06519 Cyclic Olefinic Copolymer (Asia Pacific)
LNP STAT-KON* 9X06519 is a compound based on Cyclic Olefinic Copolymer resin containing Carbon Fiber. Added features of this material include: Clean Compounding System.