Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 70.0 - 130 µm/m-°C
38.9 - 72.2 µin/in-°F
Average value: 111 µm/m-°C Grade Count:16
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an..
CTE, linear, Transverse to Flow 86.4 - 130 µm/m-°C
48.0 - 72.2 µin/in-°F
Average value: 101 µm/m-°C Grade Count:25
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
CTE, linear, Transverse to Flow 78.0 - 130 µm/m-°C
43.3 - 72.2 µin/in-°F
Average value: 103 µm/m-°C Grade Count:3
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
CTE, linear, Transverse to Flow 68.0 - 130 µm/m-°C
37.8 - 72.2 µin/in-°F
Average value: 88.6 µm/m-°C Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..