Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 86.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
CTE, linear, Transverse to Flow | 86.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® FR15 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
CTE, linear, Transverse to Flow | 86.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
CTE, linear, Transverse to Flow | 86.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
CTE, linear, Transverse to Flow | 86.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
CTE, linear, Transverse to Flow | 86.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG38F ABS Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
CTE, linear, Transverse to Flow | 86.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG38F ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
CTE, linear, Transverse to Flow | 86.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG38N ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
CTE, linear, Transverse to Flow | 86.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG38N ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
CTE, linear, Transverse to Flow | 86.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MGABS01 ABS Injection molding ABS. High impact, high gloss, good flow. |
|||
CTE, linear, Transverse to Flow | 86.4 - 130 µm/m-°C | 48.0 - 72.2 µin/in-°F | Average value: 101 µm/m-°C Grade Count:25 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
CTE, linear, Transverse to Flow | 86.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 3706 PBT+PC Impact modified PBT+PC resin. Outdoor enclosure. Not available in all colors. |
|||
CTE, linear, Transverse to Flow | 86.4 µm/m-°C @Temperature -40.0 - 37.8 °C |
48.0 µin/in-°F @Temperature -40.0 - 100 °F |
ASTM E831 |
Diamond Polymers DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed.. |