Polymer Property : CTE, linear, Transverse to Flow = 77.2 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 139 - 158 µm/m-°C

@Temperature 55.0 - 160 °C
77.2 - 87.8 µin/in-°F

@Temperature 131 - 320 °F
Average value: 155 µm/m-°C Grade Count:5
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
CTE, linear, Transverse to Flow 139 µm/m-°C

@Temperature 23.0 - 60.0 °C
77.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp MX05039 PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MX05039 is a compound based on Polypropylene resin containing Mineral, colorant. Added features include : Heat- Stabilized, UV - Stabilized.This data was supplied by SABIC-IP for th..
CTE, linear, Transverse to Flow 139 µm/m-°C

@Temperature 20.0 °C
77.2 µin/in-°F

@Temperature 68.0 °F
Eastman Ecdel PCCE 9965 Copolyester Ether Elastomer
ISO data as provided by the manufacturer, Eastman Chemical
CTE, linear, Transverse to Flow 139 µm/m-°C

@Temperature 23.0 - 60.0 °C
77.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starpylen MX05039 PP, Mineral Filled, Injection Molding
Starpylen MX05039 is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar.