Polymer Property : CTE, linear = 10.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 17.0 - 18.0 µm/m-°C

@Temperature 20.0 - 300 °C
9.44 - 10.0 µin/in-°F

@Temperature 68.0 - 572 °F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T6
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
CTE, linear 17.0 - 18.0 µm/m-°C

@Temperature 20.0 - 300 °C
9.44 - 10.0 µin/in-°F

@Temperature 68.0 - 572 °F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
CTE, linear 17.0 - 18.0 µm/m-°C

@Temperature 20.0 - 300 °C
9.44 - 10.0 µin/in-°F

@Temperature 68.0 - 572 °F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T4
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..