Thermal Properties Metric English Comments
CTE, linear 11.18 µm/m-°C

@Temperature 20.0 - 200 °C
6.211 µin/in-°F

@Temperature 68.0 - 392 °F
Crucible Steel CPM® 9V® Tool Steel
CPM 9V is made by the Crucible Particle Metallurgy process. Its composition is a modification of CPM 10V with lower carbon and vanadium to improve toughness and heat check resistance. These enhanced..
CTE, linear 11.18 µm/m-°C

@Temperature 20.0 - 205 °C
6.211 µin/in-°F

@Temperature 68.0 - 401 °F
Crucible Steel CPM® Rex® 20® (HS) High Speed Steel
CPM Rex 20 is a cobalt-free super high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It has heat treat response and red hardness comparable to that of M42 but offers better wea..
CTE, linear 11.18 µm/m-°C

@Temperature 24.0 - 538 °C
6.211 µin/in-°F

@Temperature 75.2 - 1000 °F
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications
Description: Ferrium® S53® is a corrosion resistant ultra high-strength steel for structural aerospace applications. Ferrium® S53® was designed to provide mechanical properties equal to, or bett..