Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 260 °C |
6.22 µin/in-°F @Temperature 68.0 - 500 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 1.25 RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 260 °C |
6.22 µin/in-°F @Temperature 68.0 - 500 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 2.25" RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 260 °C |
6.22 µin/in-°F @Temperature 68.0 - 500 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 3" RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 316 °C |
6.22 µin/in-°F @Temperature 68.0 - 601 °F |
|
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked Solution Treated, 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 316 °C |
6.22 µin/in-°F @Temperature 68.0 - 601 °F |
|
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 400 °C |
6.22 µin/in-°F @Temperature 68.0 - 752 °F |
DIN EN 821-1 |
CeramTec MZ 111 Zirconia, ZrO2-Y2O3 MZ 111 is a yttria-stabilized tetragonal zirconia used in dental applications. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 400 °C |
6.22 µin/in-°F @Temperature 68.0 - 752 °F |
DIN EN 821-1 |
CeramTec MZ 429 Zirconia, ZrO2-Y2O3 MZ 429 is a yttria-stabilized zirconia ceramic. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 38.0 - 260 °C |
6.22 µin/in-°F @Temperature 100 - 500 °F |
|
Crucible Compaction Metals CPM® VIM CRU® 20® CPM® VIM CRU® 20® is a vacuum induction melted, cobalt-free super high speed steel manufactured by the Crucible Particle Metallurgy (CPM®) process. VIM CRU processing is designed to meet the cle.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 21.1 - 200 °C |
6.20 µin/in-°F @Temperature 70.0 - 392 °F |
|
Crucible Steel KAPSTAR® Mold Steel Kapstar is a high hard, precipitation hardening mold steel suitable for production of machined or EDM’d plastic mold, rubber mold, and zinc die casting die components. Kapstar is supplied at about .. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 37.8 - 427 °C |
6.24 µin/in-°F @Temperature 100 - 800 °F |
|
Crucible Steel REX® M4 High Speed Steel REX M4 is a special purpose high speed steel designed to give high wear resistance in tools. Its high vanadium and carbon content provide for high resistance to cratering and wear in cold work punch.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 200 °C |
6.20 µin/in-°F @Temperature 68.0 - 392 °F |
high temp. tempering, hardened to 62 HRC |
Bohler-Uddeholm AISI D2 Cold Work Tool Steel AISI D2 is a high-carbon, high-chromium tool steel alloyed with molybdenum and vanadiumAISI AD2 is characterized by: High wear resistance High compressive strength Good through-hardening properties.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 98.9 °C |
6.22 µin/in-°F @Temperature 68.0 - 210 °F |
|
Bohler-Uddeholm BÖHLER K340 ISODUR® Premium Cold Work Steel BÖHLER K340 ISODUR is a universal cold work tool steel with which you‘ll be making money and just when blanking coins, but also when: blanking, cutting, cold rolling, extruding, deep drawing and b.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 600 °C |
6.22 µin/in-°F @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER S290 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 400 °C |
6.22 µin/in-°F @Temperature 752 °F |
|
Bohler-Uddeholm BÖHLER S590 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 199 °C |
6.20 µin/in-°F @Temperature 390 °F |
hardness of 60 HRC |
Bohler-Uddeholm UDDEHOLM VANADIS 6 Cold Work Tool Steel Description: Chromium-molybdenum-vanadium alloyed PM steel. Toolmaking with highly alloyed tool steel means that machining and heat treatment have to be considered more than with lower alloyed grade.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 22.0 - 260 °C |
6.22 µin/in-°F @Temperature 71.6 - 500 °F |
|
Carpenter Custom 450® Stainless Steel, 25 mm Bar, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 200 °C |
6.22 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum 420 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 200 °C |
6.22 µin/in-°F @Temperature 392 °F |
|
Ceramic Process Systems AlSiC-10, 54 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 22.0 - 260 °C |
6.22 µin/in-°F @Temperature 71.6 - 500 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 22.0 - 260 °C |
6.22 µin/in-°F @Temperature 71.6 - 500 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 21.0 - 316 °C |
6.22 µin/in-°F @Temperature 69.8 - 601 °F |
|
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Annealed Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 200 °C |
6.22 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 288°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 200 °C |
6.22 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 538°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 200 °C |
6.22 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 649°C (1200°F) Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 200 °C |
6.22 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420HC Allegheny Ludlum Type 420HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 22.0 - 260 °C |
6.22 µin/in-°F @Temperature 71.6 - 500 °F |
|
Carpenter Custom 455® Stainless Steel, Annealed, 25 mm Bar Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.20 µin/in-°F @Temperature 70.0 - 200 °F |
|
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel Description: Formadur 2083 Superclean is an electro slag remelted (ESR) martensitic stainless steel developed for corrosion resistant applications and Supplied in the annealed conditionCharacteristi.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 200 °C |
6.22 µin/in-°F @Temperature 68.0 - 392 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 204°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 100 °C |
6.22 µin/in-°F @Temperature 68.0 - 212 °F |
|
Industeel CREUSABRO® 8000 High Performance Wear Resistant Steel Description: CREUSABRO® 8000 is a high performance wear resistant steel, exhibiting a wear resistance of 50% higher than that of conventional 500 HB water quenched steel. CREUSABRO® 8000 is using .. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 260 °C |
6.22 µin/in-°F @Temperature 68.0 - 500 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 6" RCS High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800°.. |