Carpenter Custom 450® Stainless Steel, 25 mm Bar, Condition H1050 (Age Hardened 566°C)

Category Metal , Ferrous Metal , Stainless Steel , T 400 Series Stainless Steel
Manufacturer Carpenter Technology Corporation (Cartech)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carpenter Custom 450® Stainless Steel, 25 mm Bar, Condition H1050 (Age Hardened 566°C).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless Type 304) with moderate strength (similar to that of Stainless Type 410). the alloy has a yield strength somewhat greater than 100 ksi (689 MPa) in the annealed condition, but is easily fabricated. A single-step aging treatment develops higher strength with good ductility and toughness. This stainless can be machined, hot-worked, and cold-formed in the same manner as other martensitic age-hardenable stainless steels. A particular advantage is ease of welding and brazing. Custom 450 stainless is generally supplied in the annealed condition, requiring no heat treatment by the user for many applications. Because it has corrosion resistance like Type 304 stainless but three times the yield strength, it has been used in applications where Type 304 was not strong enough. On the other hand, it has also replaced Type 410 stainless directly on a strength basis where Type 410 had insufficient corrosion resistance. Mechanical properties will depend on the aging temperature selected.Custom 450® is a registered trademark of Carpenter Technology Corporation.
Physical Properties Metric English Comments
Density 7.76 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 369
369
Estimated from Rockwell C for 3000 kg load, 10 mm ball Brinell measurement.
Hardness, Knoop 403
403
Estimated from Rockwell C
Hardness, Rockwell C 40
40
Hardness, Vickers 386
386
Estimated from Rockwell C
Tensile Strength, Ultimate 1310 MPa
190000 psi
Tensile Strength, Yield 1207 MPa

@Strain 0.200 %
175100 psi

@Strain 0.200 %
Elongation at Break 15 %
15 %
In 4D
Reduction of Area 55 %
55 %
Modulus of Elasticity 200 GPa
29000 ksi
Poissons Ratio 0.30
0.30
Fatigue Strength 590 MPa

@# of Cycles 1.00e+7
85600 psi

@# of Cycles 1.00e+7
R.R. Moore Test, Smooth Rotating Beam
Shear Modulus 76.9 GPa
11200 ksi
Calculated
Charpy Impact 48.0 J
35.4 ft-lb
V-notch
Thermal Properties Metric English Comments
CTE, linear 10.6 µm/m-°C

@Temperature 22.0 - 93.0 °C
5.89 µin/in-°F

@Temperature 71.6 - 199 °F
11.2 µm/m-°C

@Temperature 22.0 - 260 °C
6.22 µin/in-°F

@Temperature 71.6 - 500 °F
12.0 µm/m-°C

@Temperature 22.0 - 482 °C
6.67 µin/in-°F

@Temperature 71.6 - 900 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.050 %
<= 0.050 %
min. Nb content = 8 x C content
Chromium, Cr 14 - 16 %
14 - 16 %
Copper, Cu 1.25 - 1.75 %
1.25 - 1.75 %
Iron, Fe 75 %
75 %
as remainder
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo 0.50 - 1.0 %
0.50 - 1.0 %
Nickel, Ni 5.0 - 7.0 %
5.0 - 7.0 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000758 ohm-cm

@Temperature 23.0 °C
0.0000758 ohm-cm

@Temperature 73.4 °F